MEG 309 · Basic Metallurgy and Materials Selection
Our notes
2 min readWhat corrosion is
The deterioration of a metal by chemical or electrochemical reaction with its environment. It returns refined metals towards their stable oxides, like ores.
The corrosion cell
Four parts are needed:
- Anode: metal oxidises and dissolves: Fe → Fe²⁺ + 2e⁻.
- Cathode: electrons are consumed: O₂ + 2H₂O + 4e⁻ → 4OH⁻ (in neutral water), or 2H⁺ + 2e⁻ → H₂ (in acid).
- Electrolyte: water with dissolved ions.
- Metallic path: for electrons from anode to cathode.
Remove any one and corrosion stops.
Rust
Fe²⁺ + 2OH⁻ → Fe(OH)₂, then oxidised further to hydrated Fe₂O₃ (rust).
The galvanic series
A ranking of metals in sea water. When two different metals touch in an electrolyte, the more active one corrodes faster.
| More active (anodic) | → | More noble (cathodic) |
|---|---|---|
| Magnesium, zinc, aluminium, steel, cast iron | lead, tin, brass, copper | stainless steel (passive), titanium, gold |
Worked example: area effect
Steel rivets in a copper sheet in sea water: the small steel anode is joined to a large copper cathode, so the rivets corrode fast. Copper rivets in a steel sheet: the small cathode and large anode give slow, spread-out corrosion. Avoid small anodes and large cathodes.
Forms of corrosion
| Form | Description | Example |
|---|---|---|
| Uniform | Even thinning | Rusting roof |
| Galvanic | Two metals in contact | Steel bolts in copper |
| Pitting | Deep local pits | Stainless steel in chloride |
| Crevice | Under gaskets, deposits | Flange joints |
| Intergranular | Along grain boundaries | Badly welded stainless steel |
| Stress corrosion cracking | Cracks from stress + environment | Pipelines, boilers |
| Erosion-corrosion | Flow wears away protective films | Pump impellers, pipe bends |
| Microbial (MIC) | Bacteria, such as sulphate reducers | Oil pipelines, tanks |
Environments that speed corrosion
High humidity, salt (coastal Niger Delta), acid gases (CO₂ and H₂S in oil and gas), higher temperature, and polluted air. Port Harcourt's warm, humid, salty air is harsh on unprotected steel.
Corrosion rate
CR (mm/year) = 87.6 × W ÷ (ρ A t)
W: mass loss in mg; ρ: density in g/cm³; A: area in cm²; t: time in hours.
Worked example
A steel coupon (ρ = 7.87 g/cm³, A = 50 cm²) loses 200 mg in 30 days (720 h).
CR = 87.6 × 200 ÷ (7.87 × 50 × 720) = 17,520 ÷ 283,320 ≈ 0.062 mm/year.
Check: 0.062 mm = 0.0062 cm; volume lost in a year = 0.0062 × 50 = 0.31 cm³ = 2.44 g. Over 30 days: 2.44 × 30 ÷ 365 ≈ 0.20 g = 200 mg. Correct.
High-temperature oxidation
Without water, metals react directly with oxygen at high temperature, forming scale. The Pilling-Bedworth ratio (oxide volume ÷ metal volume) helps predict protection: a ratio a little above 1 gives a protective, adherent film (as in aluminium); much higher or lower gives cracked or porous scale.
Exams usually ask
- Describe the electrochemical corrosion cell.
- Explain galvanic corrosion and the area effect.
Common mistake
Thinking the more noble metal corrodes in a galvanic couple. The more active metal corrodes.
Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.
Read
-
Best pick Chemistry 2e, 17.6 Corrosion
(opens openstax.org in a new tab)
OpenStax, Chemistry 2e, 17.6 Corrosion, CC BY-NC-SA 4.0 · licence
-
Corrosion
(opens en.wikipedia.org in a new tab)
Wikipedia, Corrosion, CC BY-SA 4.0 · licence
-
Galvanic corrosion
(opens en.wikipedia.org in a new tab)
Wikipedia, Galvanic corrosion, CC BY-SA 4.0 · licence
-
OpenStax, Chemistry 2e (whole free textbook)
The whole book, free to read online or download as a PDF (the PDF is large: Wi-Fi).
(opens openstax.org in a new tab)
OpenStax, OpenStax, Chemistry 2e (whole free textbook), CC BY-NC-SA 4.0 · licence
-
NOUN CHM 409: Electrochemistry
NOUN course book (PDF, about 3.2 MB). The electrochemistry behind corrosion.
(opens nou.edu.ng in a new tab)
Watch
-
Electrochemistry: Crash Course Chemistry #36
9 min · ≈ 41 MB · about ₦23
(opens youtube.com in a new tab)
-
Electrochemistry
6 min · ≈ 27 MB · about ₦15
(opens youtube.com in a new tab)
-
GCSE Chemistry - What is Corrosion and How to Stop it (2026/27 exams)
6 min · ≈ 27 MB · about ₦15
(opens youtube.com in a new tab)
-
Electrochemistry Review - Cell Potential & Notation, Redox Half Reactions, Nernst Equation
1 h 27 min · ≈ 392 MB · about ₦220
(opens youtube.com in a new tab)
We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.