MEG 309 · Basic Metallurgy and Materials Selection
Our notes
2 min readApproaches
Attack any part of the corrosion cell: the metal, the environment, the electrical path, or the surface.
Good design
- Avoid crevices, pockets and water traps; allow drainage.
- Avoid joining dissimilar metals, or insulate them.
- Avoid small anodes with large cathodes.
- Allow access for inspection and painting.
- Add a corrosion allowance: extra thickness to be lost over the design life.
Material choice
Stainless steels, aluminium, copper alloys, plastics or composites where corrosion is severe.
Coatings
| Type | Examples | How it protects |
|---|---|---|
| Paint | Primer + topcoats | Barrier |
| Metallic, sacrificial | Galvanising (zinc) | Barrier, and zinc corrodes first |
| Metallic, noble | Tin, chromium, nickel | Barrier only: fails if scratched |
| Conversion | Phosphating, anodising (aluminium) | Thin protective layer |
| Pipeline coatings | Fusion-bonded epoxy, polyethylene | Barrier |
Surface preparation (removing rust and mill scale, often by blasting) decides how long a coating lasts.
Cathodic protection
Make the whole structure a cathode:
- Sacrificial anodes: zinc, aluminium or magnesium blocks attached to the steel corrode instead: ship hulls, jetties, buried pipelines.
- Impressed current: a DC power source with inert anodes drives current onto the structure: long pipelines and large structures.
Coatings and cathodic protection are used together: the coating does most of the work, CP protects the gaps.
Inhibitors
Chemicals added in small amounts to a liquid to slow corrosion: in boiler water, cooling systems, oil and gas pipelines and radiator coolant.
Environment control
- Remove oxygen from boiler water.
- Control pH.
- Dehumidify air.
Measuring and monitoring
| Method | How |
|---|---|
| Weight-loss coupons | Weigh, expose, clean, re-weigh (see the rate formula) |
| Electrical resistance (ER) probes | Resistance rises as the element thins |
| Linear polarisation resistance (LPR) | Electrochemical rate in conducting liquids |
| Ultrasonic thickness (UT) | Measures remaining wall thickness from outside |
| Pipeline pigs (intelligent) | Travel inside pipelines and map metal loss |
| CP surveys | Measure pipe-to-soil potential |
| Visual inspection | Simple and vital |
Worked example: remaining life
A pipe wall was 12.0 mm; a UT survey now reads 9.6 mm after 8 years. The minimum allowed thickness is 6.0 mm.
Rate = (12.0 − 9.6) ÷ 8 = 0.30 mm/year.
Remaining life = (9.6 − 6.0) ÷ 0.30 = 12 years.
Check: 9.6 − 12 × 0.30 = 9.6 − 3.6 = 6.0 mm. Correct. Plan inspection well before then, since rates can change.
Cost of corrosion
Studies in several countries estimate the cost of corrosion at a few percent of GDP, with much of it avoidable by known methods. Pipeline leaks in the Niger Delta add environmental and social costs.
Exams usually ask
- Explain sacrificial and impressed-current cathodic protection.
- Describe three methods of corrosion monitoring.
Common mistake
Relying on a noble coating such as tin over steel with scratches. At a scratch the steel is the anode and corrodes faster.
Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.
Read
-
Cathodic protection
(opens en.wikipedia.org in a new tab)
Wikipedia, Cathodic protection, CC BY-SA 4.0 · licence
-
Galvanization
(opens en.wikipedia.org in a new tab)
Wikipedia, Galvanization, CC BY-SA 4.0 · licence
-
Corrosion inhibitor
(opens en.wikipedia.org in a new tab)
Wikipedia, Corrosion inhibitor, CC BY-SA 4.0 · licence
-
Sacrificial metal
(opens en.wikipedia.org in a new tab)
Wikipedia, Sacrificial metal, CC BY-SA 4.0 · licence
-
NOUN CHM 409: Electrochemistry
NOUN course book (PDF, about 3.2 MB). The electrochemistry behind corrosion.
(opens nou.edu.ng in a new tab)
Watch
-
Best pick Ship Hull Protection System
8 min · ≈ 36 MB · about ₦20
(opens youtube.com in a new tab)
-
Corrosion prevention - Impressed current cathodic protection
4 min · ≈ 18 MB · about ₦10
(opens youtube.com in a new tab)
-
Cathodic Protection Explained — Complete Beginner’s Guide
16 min · ≈ 72 MB · about ₦40
(opens youtube.com in a new tab)
-
Cathodic Protection Criteria and Pipe-to-Soil Potentials
38 min · ≈ 171 MB · about ₦96
(opens youtube.com in a new tab)
We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.