MEG 309 · Basic Metallurgy and Materials Selection

Heat treatment of steels

Annealing, normalising, hardening, tempering and case hardening, TTT diagrams, and the equipment used.

Our notes

2 min read

What heat treatment does

Controlled heating and cooling changes the microstructure, and so the properties, without changing the shape.

Main processes

ProcessHeat toCoolResult
Full annealingAbout 30-50°C above A₃Very slowly in the furnaceSoft, ductile; coarse pearlite; relieves stresses
NormalisingAbout 30-50°C above A₃ (or A_cm)In still airFiner pearlite; stronger than annealed; uniform structure
HardeningAbove A₃ (austenite)Quench in water, oil or brineMartensite: very hard, brittle
TemperingBelow A₁ (often 150-650°C)AirReduces brittleness; trades hardness for toughness
Stress relievingBelow A₁SlowlyRemoves stresses from welding or machining

Martensite

Fast cooling traps carbon in a distorted (body-centred tetragonal) iron lattice. It is very hard, and the harder the more carbon (up to a limit). Low-carbon steels (under about 0.3% C) do not harden much by quenching.

TTT diagrams

Time-temperature-transformation diagrams show, for a given steel, how austenite transforms at constant temperature: to pearlite (slow, high temperatures), bainite (intermediate) or martensite (below the M_s line, fast cooling). The nose of the curve shows how fast you must cool to avoid pearlite.

Hardenability

The depth to which a steel can be hardened. Alloying elements (Cr, Mo, Ni, Mn) increase it. Measured by the Jominy end-quench test.

Quenching media

MediumSpeedRisk
BrineFastestCracking, distortion
WaterFastCracking in high-carbon steel
OilSlowerLess cracking; for alloy steels
AirSlowestOnly for highly alloyed (air-hardening) steels

Case hardening

Hard surface for wear, tough core for shock: gears, cams, pins.

  • Carburising: heat low-carbon steel in a carbon-rich atmosphere, then quench.
  • Nitriding: diffuse nitrogen at lower temperature; little distortion.
  • Flame or induction hardening: heat only the surface of a medium-carbon steel, then quench.

Equipment

  • Furnaces: electric or gas, box or pit type, sometimes with controlled atmosphere to prevent scaling and decarburisation.
  • Salt baths: even heating.
  • Quench tanks with agitation.
  • Temperature measurement: thermocouples and pyrometers.
  • Hardness testers for checking results.

In small workshops, colours of heated steel are used as rough guides, but they are not accurate.

Worked example: holding time

A common workshop rule is about 1 hour of soaking per 25 mm of section thickness (a rule of thumb; follow the specification). A 75 mm shaft: 75 ÷ 25 = 3 hours.
Check: 3 × 25 = 75. Correct.

Safety

Hot metal, quench oil fires, salt bath splashes: wear protective clothing and keep fire equipment near.

Exams usually ask

  • Distinguish annealing, normalising, hardening and tempering.
  • Explain the purpose of a TTT diagram.

Common mistake

Using a hardened part without tempering. Untempered martensite is brittle and may crack in service.

Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.

Read

Watch

We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.

All MEG 309 topics

Report

Sign in to report this. It is free.

Is this your work (a lecturer, author or publisher)? Ask us to take it down.