ENG 204 · Basic Engineering Materials
Our notes
2 min readPurpose
Heat treatment changes the microstructure, and therefore the properties, of a metal without changing its shape: to soften for machining, relieve stresses, refine grains, harden or toughen.
Time-temperature-transformation (TTT) diagrams
For a eutectoid steel cooled quickly to a temperature and held:
- Just below 727 °C: coarse pearlite (soft).
- Around 550-600 °C (the "nose", fastest transformation): fine pearlite.
- About 250-550 °C: bainite (fine ferrite and cementite needles; strong and tough).
- Below M_s (about 220 °C for eutectoid steel): martensite, formed without diffusion.
Continuous cooling (CCT) diagrams are used for real cooling.
Martensite
Austenite quenched fast enough to miss the pearlite nose transforms by shear to martensite: a supersaturated solution of carbon in a distorted (body-centred tetragonal) iron lattice. Very hard and brittle; hardness rises with carbon. The critical cooling rate is the slowest cooling that gives full martensite.
The main treatments
| Treatment | Process | Result |
|---|---|---|
| Full annealing | heat about 30-50 °C above the upper critical line (hypoeutectoid), hold, cool slowly in the furnace | coarse pearlite; soft, ductile, machinable |
| Process annealing | heat below 727 °C (550-650 °C) | removes cold-work hardening (recrystallisation) |
| Stress relieving | heat to moderate temperature, cool slowly | removes residual stresses from welding or machining |
| Spheroidising | long hold just below 727 °C | cementite as spheres; best machinability for high-carbon steels |
| Normalising | heat above the upper critical line, cool in still air | finer pearlite, uniform grain; stronger than annealed |
| Hardening (quenching) | austenitise, quench in water, brine or oil | martensite; very hard, brittle |
| Tempering | reheat quenched steel to 150-650 °C | tempered martensite; less brittle, tougher; higher temperature, softer |
Hardenability
The ability of a steel to form martensite to a depth on quenching (not the maximum hardness). Raised by alloying elements (Cr, Mo, Ni, Mn). Measured by the Jominy end-quench test.
Surface (case) hardening
A hard, wear-resistant surface with a tough core:
- Carburising: add carbon by diffusion at about 900-950 °C, then quench and temper (gears).
- Nitriding: nitrogen at about 500-550 °C; no quench needed.
- Carbonitriding, cyaniding.
- Flame and induction hardening: heat only the surface of a medium-carbon steel and quench.
Exams usually ask
- Explain the TTT diagram and the products of different cooling paths.
- Describe annealing, normalising, hardening and tempering, and their purposes.
- Distinguish hardness from hardenability; describe case hardening.
Common mistake
Quenching without tempering. As-quenched martensite is too brittle for most uses; tempering is almost always the next step.
Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.
Read
-
Best pick Heat treating
(opens en.wikipedia.org in a new tab)
Wikipedia, Heat treating, CC BY-SA 4.0 · licence
-
Quenching
(opens en.wikipedia.org in a new tab)
Wikipedia, Quenching, CC BY-SA 4.0 · licence
-
Annealing (materials science)
(opens en.wikipedia.org in a new tab)
Wikipedia, Annealing (materials science), CC BY-SA 4.0 · licence
Watch
-
10 Misconceptions About Heat Treating Steel
18 min · ≈ 81 MB · about ₦45
(opens youtube.com in a new tab)
-
Elements of Tempering, Normalizing, and Annealing
14 min · ≈ 63 MB · about ₦35
(opens youtube.com in a new tab)
-
How to Harden and Temper 4140 Medium Carbon Steel
11 min · ≈ 50 MB · about ₦28
(opens youtube.com in a new tab)
-
Heat Treating Steel
5 min · ≈ 23 MB · about ₦13
(opens youtube.com in a new tab)
We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.