ENG 204 · Basic Engineering Materials
Our notes
2 min readFatigue
Failure under repeated (cyclic) stresses below the static strength. It causes most service failures of machine parts: shafts, springs, aircraft parts, bridges, crankshafts.
Stress cycles
- Mean stress σ_m = (σ_max + σ_min)/2.
- Stress amplitude σ_a = (σ_max − σ_min)/2.
- Range Δσ = σ_max − σ_min.
- Stress ratio R = σ_min/σ_max (fully reversed: R = −1).
Example: σ_max = 200 MPa, σ_min = −50 MPa: σ_m = 75 MPa, σ_a = 125 MPa, R = −0.25.
S-N curve
Stress amplitude against the number of cycles to failure (log scale).
- Steels and titanium: the curve flattens at a fatigue (endurance) limit, roughly 0.35 to 0.5 × UTS for steels; below it the part lasts indefinitely.
- Aluminium, copper: no limit; a fatigue strength at a stated number of cycles (often 10⁷ or 10⁸) is quoted.
Stages of fatigue failure
- Crack initiation at a stress raiser (notch, hole, scratch, inclusion, sharp corner).
- Slow crack growth, leaving beach marks and striations.
- Sudden final fracture of the remaining section.
Improving fatigue life
Smooth surfaces and generous fillets, avoiding sharp changes of section, shot peening or surface rolling (compressive surface stresses), case hardening, avoiding corrosion (corrosion fatigue).
Creep
Slow, time-dependent plastic deformation under constant load at high temperature, usually above about 0.4 T_m (absolute melting temperature). Important in boilers, steam and gas turbines, jet engines, furnace parts.
The creep curve (strain against time)
- Instantaneous strain on loading.
- Primary creep: decreasing rate (work hardening).
- Secondary (steady-state) creep: constant minimum rate, the longest stage, used in design.
- Tertiary creep: accelerating; necking, voids, rupture.
Higher stress or temperature raises the steady creep rate and shortens rupture life.
Example: 0.4 T_m
Lead melts at 600 K: 0.4 T_m = 240 K, so lead creeps at room temperature (old lead pipes sag). Steel (T_m about 1,800 K): creep matters above about 450 °C.
Creep-resistant materials
High melting point, coarse grains or single crystals (turbine blades), stable precipitates and solid solution strengthening: nickel superalloys, Cr-Mo steels in power plant pipes, ceramics.
Exams usually ask
- Explain fatigue, the S-N curve and the endurance limit; describe a fatigue fracture surface.
- Calculate mean stress, amplitude and stress ratio.
- Sketch and explain the creep curve; list ways of improving creep resistance.
Common mistake
Thinking fatigue happens only at high stress. It happens at stresses well below the yield strength if they are repeated many times.
Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.
Read
-
Creep (deformation)
(opens en.wikipedia.org in a new tab)
Wikipedia, Creep (deformation), CC BY-SA 4.0 · licence
-
Fatigue (material)
(opens en.wikipedia.org in a new tab)
Wikipedia, Fatigue (material), CC BY-SA 4.0 · licence
Watch
-
Best pick Mechanics of Materials: Lesson 16 - Fatigue and Creep Failures with S-N Diagram
7 min · ≈ 32 MB · about ₦18
(opens youtube.com in a new tab)
-
Materials Science Explained: Stress-Strain Curve, Fatigue & Why Materials Fail
8 min · ≈ 36 MB · about ₦20
(opens youtube.com in a new tab)
-
Fatigue Failure
7 min · ≈ 32 MB · about ₦18
(opens youtube.com in a new tab)
-
Static Loading and the Effects of Creep
6 min · ≈ 27 MB · about ₦15
(opens youtube.com in a new tab)
-
Lecture 26 : Creep Fundamentals
54 min · ≈ 243 MB · about ₦136
(opens youtube.com in a new tab)
We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.