UNIHIVE

Study Hub UNIPORT MEG 309

MEG 309 · Basic Metallurgy and Materials Selection

Crystal structure and mechanical properties

BCC, FCC and HCP, defects, and the tensile test and other property measurements.

Our notes

2 min read

Crystal structures of metals

StructureAtoms per cellPacking factorExamples
Body-centred cubic (BCC)20.68Iron below 912°C (ferrite), chromium, tungsten
Face-centred cubic (FCC)40.74Aluminium, copper, nickel, iron 912-1,394°C (austenite)
Hexagonal close-packed (HCP)6 (per hexagonal cell)0.74Zinc, titanium, magnesium

FCC metals are generally ductile, even at low temperature. BCC metals (such as ordinary steel) can turn brittle when cold. HCP metals have fewer easy slip systems and are less formable.

Worked example: density of iron

BCC iron: lattice parameter a = 0.2866 nm, 2 atoms per cell, M = 55.85 g/mol.
Cell volume = (0.2866 × 10⁻⁷ cm)³ = 2.354 × 10⁻²³ cm³.
Mass in cell = 2 × 55.85 ÷ 6.022 × 10²³ = 1.855 × 10⁻²² g.
Density = 1.855 × 10⁻²² ÷ 2.354 × 10⁻²³ ≈ 7.88 g/cm³.
Check: measured density of iron is about 7.87 g/cm³. Agrees.

Allotropy

Iron changes structure with temperature: BCC (α) to FCC (γ) at 912°C, back to BCC (δ) at 1,394°C, melting at 1,538°C. This change is what makes steel heat-treatable.

Defects

  • Point: vacancies, interstitial atoms (carbon in iron), substitutional atoms.
  • Line: dislocations: their movement lets metals deform plastically.
  • Planar: grain boundaries.

Anything that blocks dislocations makes a metal stronger: small grains, alloy atoms, precipitates, cold work.

The tensile test

A standard specimen is pulled until it breaks.

PropertyMeaning
Young's modulus EStiffness: stress ÷ strain in the elastic region
Yield strengthStress at which permanent deformation begins
Tensile strength (UTS)Highest stress reached
Elongation% stretch at fracture: ductility
Reduction of areaAnother ductility measure

Worked example

A steel bar of 10 mm diameter yields at 23.6 kN.
Area = π × 10² ÷ 4 = 78.54 mm². Yield strength = 23,600 ÷ 78.54 ≈ 300 MPa (N/mm²).
Check: 300 × 78.54 = 23,562 N ≈ 23.6 kN. Correct.

Other tests

  • Hardness: Brinell, Vickers, Rockwell: resistance to indentation; roughly linked to strength.
  • Impact (Charpy): energy absorbed in breaking a notched bar; shows the brittle transition in BCC steels.
  • Fatigue: repeated loading below the yield strength can cause failure; most service failures of shafts and springs are fatigue.
  • Creep: slow deformation under load at high temperature.

Exams usually ask

  • Compare BCC, FCC and HCP structures.
  • Calculate stress, strain and yield strength from test data.

Common mistake

Confusing strength and stiffness. Stiffness is E; a high-strength steel has almost the same E as a mild steel.

Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.

Read

Watch

We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.

All MEG 309 topics

Report

Sign in to report this. It is free.

Is this your work (a lecturer, author or publisher)? Ask us to take it down.