MEG 309 · Basic Metallurgy and Materials Selection
Our notes
2 min readWhy it matters
It shows which phases are present in iron-carbon alloys at each temperature and carbon content under slow cooling. It is the map for heat treatment.
The phases
| Phase | Structure | Notes |
|---|---|---|
| Ferrite (α) | BCC | Soft, ductile; dissolves very little carbon (up to about 0.022%) |
| Austenite (γ) | FCC | Stable at high temperature; dissolves up to about 2.1% C; non-magnetic |
| Cementite (Fe₃C) | Compound, 6.67% C | Hard and brittle |
| Liquid |
Key points
| Point | Temperature | Carbon |
|---|---|---|
| Eutectoid | 727°C | about 0.76% |
| Eutectic | 1,148°C | 4.3% |
| Maximum C in austenite | 1,148°C | about 2.1% |
The eutectoid reaction
On slow cooling through 727°C: austenite (0.76% C) → ferrite + cementite, as fine alternating plates called pearlite.
Steels and cast irons
- Steel: up to about 2.1% C.
- Hypoeutectoid (below 0.76%): ferrite + pearlite.
- Eutectoid (0.76%): all pearlite.
- Hypereutectoid (0.76 to 2.1%): pearlite + cementite at the grain boundaries.
- Cast iron: above about 2.1% C.
Critical temperatures
- A₁: 727°C, the eutectoid line.
- A₃: where ferrite starts to form on cooling in hypoeutectoid steel.
- A_cm: where cementite starts to form in hypereutectoid steel.
These guide annealing and hardening temperatures.
The lever rule
In a two-phase region, the fraction of each phase is found from a horizontal tie line:
fraction of phase A = (distance from the alloy to phase B) ÷ (total tie-line length).
Worked example
A 0.40% C steel just below 727°C. What fraction is pearlite?
Just above 727°C the steel is proeutectoid ferrite (0.022%) + austenite (0.76%); the austenite becomes pearlite.
Pearlite fraction = (0.40 − 0.022) ÷ (0.76 − 0.022) = 0.378 ÷ 0.738 ≈ 0.51 (51%).
Ferrite (proeutectoid) = 1 − 0.51 = 0.49.
Check with a carbon balance: 0.49 × 0.022 + 0.51 × 0.76 = 0.0108 + 0.3876 ≈ 0.398 ≈ 0.40%. Correct.
Effect of carbon on properties
| Carbon | Strength and hardness | Ductility | Typical use |
|---|---|---|---|
| Low (under 0.25%) | Lower | High | Sheets, wire, rebar, structural sections |
| Medium (0.25 to 0.6%) | Medium | Medium | Shafts, gears, rails |
| High (over 0.6%) | High | Low | Springs, cutting tools, knives |
Limits of the diagram
It applies to slow (equilibrium) cooling and plain iron-carbon alloys. Fast cooling gives non-equilibrium structures such as martensite, shown on TTT and CCT diagrams instead. Alloying elements shift the lines.
Exams usually ask
- Sketch the steel part of the diagram and label phases and key points.
- Use the lever rule to find phase fractions.
Common mistake
Reading the lever rule the wrong way round. The fraction of a phase uses the length of the tie line on the opposite side of the alloy.
Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.
Read
-
Austenite
(opens en.wikipedia.org in a new tab)
Wikipedia, Austenite, CC BY-SA 4.0 · licence
-
Pearlite
(opens en.wikipedia.org in a new tab)
Wikipedia, Pearlite, CC BY-SA 4.0 · licence
-
Cementite
(opens en.wikipedia.org in a new tab)
Wikipedia, Cementite, CC BY-SA 4.0 · licence
Watch
-
Best pick Iron-Carbon Phase Diagram simply explained Part II | Microstructure | hypo- & hypereutectoid
21 min · ≈ 95 MB · about ₦53
(opens youtube.com in a new tab)
-
Iron Carbon Phase Diagram
8 min · ≈ 36 MB · about ₦20
(opens youtube.com in a new tab)
-
Steel phase diagram cooling and Lever Rule example problem
8 min · ≈ 36 MB · about ₦20
(opens youtube.com in a new tab)
-
#62 Phase Diagrams | Iron Iron Carbide Phase Diagram | Basics of Materials Engineering
41 min · ≈ 185 MB · about ₦104
(opens youtube.com in a new tab)
We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.