No real crystal is perfect. Defects control strength, ductility, diffusion, conductivity and colour; much of materials engineering is about controlling them.
Point defects
- Vacancy: a missing atom. The equilibrium number rises sharply with temperature: N_v = N exp(−Q_v/kT).
- Self-interstitial: an extra host atom squeezed between sites (rare in metals; large distortion).
- Impurity atoms: substitutional (replace a host atom) or interstitial (sit in the gaps).
- In ionic crystals: Schottky defect (a cation-anion vacancy pair) and Frenkel defect (a cation moved to an interstitial site), keeping charge balance.
Worked example: vacancies in copper at 1,000 °C
Q_v = 0.9 eV, k = 8.62 × 10⁻⁵ eV/K, T = 1,273 K.
N_v/N = exp(−0.9/(8.62 × 10⁻⁵ × 1,273)) = exp(−8.20) ≈ 2.7 × 10⁻⁴ (about 3 vacancies per 10,000 sites).
Solid solutions
An alloying element dissolved in the host crystal without changing its structure.
- Substitutional: e.g. nickel in copper, zinc in copper (brass).
- Interstitial: small atoms (C, N, H, B) in the gaps of iron: carbon in iron makes steel.
Hume-Rothery rules for wide substitutional solubility: atomic radii within about 15%, the same crystal structure, similar electronegativity, similar valence. Copper and nickel meet all four and dissolve completely.
Line defects: dislocations
- Edge dislocation: an extra half-plane of atoms ending inside the crystal.
- Screw dislocation: a spiral ramp of atoms.
- Most are mixed.
The Burgers vector b gives the size and direction of the lattice distortion. Dislocations move under shear stress (slip), so metals deform plastically at stresses far below the theoretical strength of a perfect crystal. Anything that blocks dislocation motion makes the metal stronger: solute atoms, other dislocations (work hardening), grain boundaries, fine precipitates.
Planar (interfacial) defects
- Grain boundaries: where grains of different orientation meet. Smaller grains mean more boundary area and higher strength (Hall-Petch: σ_y = σ₀ + k_y d^(−1/2)).
- Twin boundaries: mirror-image arrangements.
- Stacking faults and external surfaces.
Volume defects
Pores, cracks, inclusions (slag, oxides), and shrinkage cavities from casting. They concentrate stress and start fractures.
Grain size
Measured by the ASTM grain size number or the average grain diameter under a microscope after polishing and etching.
Exams usually ask
- Classify crystal defects with sketches.
- Distinguish edge from screw dislocations; explain the role of dislocations in plastic deformation and strengthening.
- State the Hume-Rothery rules.
Common mistake
Saying defects only weaken materials. Controlled defects (alloying atoms, fine grains, dislocations) are how metals are strengthened.
Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.
Read
-
Crystallographic defect
(opens en.wikipedia.org in a new tab)
Wikipedia, Crystallographic defect, CC BY-SA 4.0 · licence
-
Dislocation
(opens en.wikipedia.org in a new tab)
Wikipedia, Dislocation, CC BY-SA 4.0 · licence
-
Grain boundary
(opens en.wikipedia.org in a new tab)
Wikipedia, Grain boundary, CC BY-SA 4.0 · licence
Watch
-
Best pick #11 Defects in Crystalline Materials | Types of Crystalline Defects | Part 1
13 min · ≈ 59 MB · about ₦33
(opens youtube.com in a new tab)
-
Crystal Defects or Imperfections in Solids
8 min · ≈ 36 MB · about ₦20
(opens youtube.com in a new tab)
-
IMPERFECTION IN SOLIDS
4 min · ≈ 18 MB · about ₦10
(opens youtube.com in a new tab)
-
Engineering Materials: Ch4.1- 4.3 Imperfections in Solids- Point Defects
26 min · ≈ 117 MB · about ₦66
(opens youtube.com in a new tab)
-
10/5/16 Intro to MSE defects and crystalline imperfections
51 min · ≈ 230 MB · about ₦129
(opens youtube.com in a new tab)
We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.