CHM 250 · Inorganic Chemistry I
Our notes
2 min readWhy alloy
A pure metal's atoms slide over each other easily. Different-sized atoms in an alloy disturb the planes, so alloys are usually harder and stronger, often more corrosion-resistant, with lower melting points or special properties.
Types
- Substitutional solid solution: solute atoms replace host atoms (Cu-Ni, Cu-Zn brass).
- Interstitial solid solution: small atoms (C, N, H, B) sit in the gaps between host atoms (carbon in iron: steel).
- Intermetallic compounds: fixed ratios and their own structures (CuAl₂, Ni₃Al, Mg₂Si): hard, often brittle; they strengthen many alloys.
Hume-Rothery rules (for wide substitutional solubility)
- Atomic radii differ by less than about 15%.
- The same crystal structure.
- Similar electronegativity (else compounds form).
- Similar valency (a metal dissolves a higher-valent one more readily than the reverse).
Worked example 1
Cu (radius 128 pm) and Zn (134 pm): difference = 6 ÷ 128 ≈ 4.7%, under 15%, so wide solubility is expected: brass dissolves up to about 35% Zn in copper's structure ✓. Cu and Ni (about 125 pm, both face-centred cubic, similar electronegativity and valency) are completely soluble in each other at all compositions (monel).
Phase diagrams
A binary phase diagram shows which phases exist at each temperature and composition. A eutectic is the composition that melts at the lowest temperature, sharply, like a pure substance. Lead-tin: eutectic at about 61.9% Sn, 183 °C: ideal for solder.
The lever rule
In a two-phase region, draw the tie line at that temperature. Fraction of phase = length of the opposite arm ÷ total length.
Worked example 2
A Pb-Sn alloy with 40% Sn just above 183 °C contains solid α (18.3% Sn) and liquid (61.9% Sn).
Fraction liquid = (40 − 18.3) ÷ (61.9 − 18.3) = 21.7 ÷ 43.6 ≈ 0.50; fraction α ≈ 0.50.
Check the tin balance: 0.50 × 61.9 + 0.50 × 18.3 = 30.95 + 9.15 ≈ 40.1% ≈ 40% ✓.
Main-group and other common alloys
| Alloy | Composition (about) | Use |
|---|---|---|
| Solder | Sn-Pb (60/40); lead-free Sn-Ag-Cu | Electronics (lead-free rules from 2006 in the EU) |
| Duralumin | Al with Cu, Mg, Mn | Aircraft, ladders (age hardening) |
| Magnesium alloys | Mg with Al, Zn | Light car and laptop parts |
| Bronze | Cu-Sn | Bearings, statues, the Igbo-Ukwu castings (leaded bronze) |
| Brass | Cu-Zn | Taps, fittings; most of the "Benin bronzes" are in fact brass |
| Steel | Fe-C (under 2% C) | Construction (CHM 350 covers iron and steel) |
Exams usually ask: define and classify alloys; state the Hume-Rothery rules; read a simple eutectic diagram; apply the lever rule; give compositions and uses of common alloys.
Common mistake: using the near arm in the lever rule. The fraction of a phase uses the arm on the opposite side of the alloy composition.
Written by the UniHive team in our own words. Spotted a mistake? Tell us on WhatsApp.
Read
-
Alloy
(opens en.wikipedia.org in a new tab)
Wikipedia, Alloy, CC BY-SA 4.0 · licence
-
Steel
(opens en.wikipedia.org in a new tab)
Wikipedia, Steel, CC BY-SA 4.0 · licence
-
Brass
(opens en.wikipedia.org in a new tab)
Wikipedia, Brass, CC BY-SA 4.0 · licence
Watch
We link to free material and never copy it. Every link was opened by our team before it went up; video data is a rough guide at 360p.